SWG16 0Cr21Al4 / 0Cr19Al3 fecral alloy Heating Wire kanggo Redrawing

Katrangan singkat:


  • materi:wesi, krom, aluminium
  • suhu operasi terus-terusan maks:1100C
  • resistensi:1.23
  • Kapadhetan:7.35
  • elongation:> 12
  • werna:padhang utawa oksidasi
  • Detail Produk

    FAQ

    Tag produk

    SWG16 0Cr21Al4 / 0Cr19Al3 fecral alloy Heating Wire kanggo Redrawing

    Resistance Wire digawe saka Nikel Chrome Alloys, Nikel Chrome Iron Alloys, Iron Chrome Aluminium Alloys, Tembaga Nikel Alloys.

    Utamane digunakake ing pemanas, unsur pemanas lan resistor, lsp.

    NiCr 80/20, NiCr 70/30, NiCr 60/15, NiCr 35/20

    CrAl 15-5, CrAl 20-5, CrAl 25-5, lsp...

    Constantan, Alloy 30, Alloy 60, Alloy 90, lsp.

    Resistivitas listrik saka 0,02 u ohm / m-1,53 u ohm / m

    Suhu operasi saka 200 C nganti 1400 C

    Pls bebas hubungi kita yen ana pitakonan.

    NiCr:
    RESISTOHM 20, RESISTOHM 30, RESISTOHM 40, RESISTOHM 60, RESISTOHM 70, RESISTOHM 80

    FeCrAl:
    RESISTOHM 125, RESISTOHM 135, RESISTOHM 140,
    RESISTOHM 145, RESISTOHM 153

    CuNi
    Constantan, Cuprothal 5, Cuprothal 10, Cuprothal 15, Cuprothal 30, Eurica

    FeCrAl Alloy Grade Komposisi kimia %
    C P S Mn Si Cr Ni Al Fe Re liyane
    maksimal (≤)
    1Cr13Al4 0.12 0,025 0,025 0.7 ≤1.00 12.5-15.0 —- 3.5-4.5 0.1 Bal.
    0Cr15Al5 0.12 0,025 0,025 0.7 ≤1.00 14.5-15.5 —- 4.5-5.3 0.1 Bal.
    0Cr25Al5 0.06 0,025 0,025 0.7 ≤0,60 23.0-26.0 ≤0,60 4.5-6.5 0.1 Bal.
    0Cr23Al5 0.06 0,025 0,025 0.7 ≤0,60 20.5-23.5 ≤0,60 4.2-5.3 0.1 Bal.
    0Cr21Al6 0.06 0,025 0,025 0.7 ≤1.00 19.0-22.0 ≤0,60 5.0-7.0 0.1 Bal.
    0Cr21Al4 0.06 0,025 0,025 0.7 ≤1.00 21.0-23.0 ≤0,60 3.0-5.2 0.1 Bal.
    0Cr21Al6Nb 0.05 0,025 0,025 0.7 ≤0,60 21.0-23.0 ≤0,60 5.0-7.0 0.1 Bal.
    0Cr27Al7Mo2 0.05 0,025 0,025 0.7 ≤0.40 26.5-27.8 ≤0,60 6.0-7.0 0.1 Bal.

    Komposisi lan Sifat Kimia:

    Properti / Kelas NiCr 80/20 NiCr 70/30 NiCr 60/15 NiCr 35/20 NiCr 30/20
    Komposisi Kimia Utama(%) Ni Bal. Bal. 55.0-61.0 34.0-37.0 30.0-34.0
      Cr 20.0-23.0 28.0-31.0 15.0-18.0 18.0-21.0 18.0-21.0
      Fe ≤ 1.0 ≤ 1.0 Bal. Bal. Bal.
    Suhu Kerja Maks (ºC) 1200 1250 1150 1100 1100
    Resistivitas ing 20ºC
    (μ Ω · m)
    1.09 1.18 1.12 1.04 1.04
    Kapadhetan (g/cm3) 8.4 8.1 8.2 7.9 7.9
    Konduktivitas termal

    (KJ/m· h· ºC)

    60.3 45.2 45.2 43.8 43.8
    Koefisien Ekspansi Termal (α × 10-6/ºC) 18 17 17 19 19
    Titik lebur (ºC) 1400 1380 1390 1390 1390
    Elongasi (%) > 20 > 20 > 20 > 20 > 20
    Struktur Mikrografi austenit austenit austenit austenit austenit
    Sifat Magnetik nonmagnetik nonmagnetik nonmagnetik nonmagnetik nonmagnetik
    CuNi Alloys Grade Resistivitas listrik
    (20 derajatΩ
    mm² / m)
    koefisien suhu saka resistance
    (10^6/derajat)
    Kapadhetan
    g/mm²
    Maks.suhu
    (derajat)
    Titik lebur
    (derajat)
    CuNi1 0.03 < 1000 8.9 200 1085
    CuNi2 0.05 < 1200 8.9 200 1090
    CuNi6 0.10 < 600 8.9 220 1095
    CuNi8 0.12 < 570 8.9 250 1097
    CuNi10 0.15 < 500 8.9 250 1100
    CuNi14 0.20 < 380 8.9 300 1115
    CuNi19 0.25 < 250 8.9 300 1135
    CuNi22 0.30 < 160 8.9 300 1150
    CuNi30 0.35 < 100 8.9 350 1170
    CuNi34 0.40 -0 8.9 350 1180
    CuNi40 0.48 ± 40 8.9 400 1280
    CuNi44 0.50 < -6 8.9 400 1280

    Kawat Pemanas SWG16 0Cr21Al4 / 0Cr19Al3 kanggo Nggambar Ulang14 warna emas 4 2018-2-11 68 2018-2-11 595 2018-2-11 125