Komposisi kimia
sasmita | Ni% | Cu% | Al% | Ti% | Fe% | Mn% | S% | C% | Si% |
Monel K500 Kab | Min 63 | 27.0-33.0 | 2.30-3.15 | 0.35-0.85 | Max 2.0 | Max 1.5 | Maks 0,01 | Maks 0,25 | Max 0,5 |
Spesifikasi
Wangun | Standar |
Monel K-500 | UNS N05500 |
bar | ASTM B865 |
Kawat | AMS4676 |
Lembaran / piring | ASTM B865 |
Forging | ASTM B564 |
Kawat Las | ERNiCu-7 |
Sifat Fisik(20°C)
sasmita | Kapadhetan | Titik Lebur | Resistivitas listrik | Rata-rata Koefisien Ekspansi Termal | Konduktivitas termal | Panas Spesifik |
Monel K500 Kab | 8,55 g/cm3 | 1315°C-1350°C | 0,615 μΩ•m | 13.7(100°C) a/10-6°C-1 | 19.4(100°C) λ/(W/m•°C) | 418 J/kg•°C |
Sifat Mekanik(20°C Min)
Monel K-500 | Kekuwatan Tensile | Kekuwatan Ngasilake RP0,2% | Elongasi A5% |
Anil & Aged | Min. 896 MPa | Min. 586MPa | 30-20 |