Sugeng rawuh ing situs web kita!

Kawat Pemanas Tungku Listrik 1.0-10.0mm FeCr25Al5 FeCr23Al5 Cerah FeCrAl alloy Resistance Spring Wire kanggo Elemen Pemanas

Katrangan singkat:


  • Nomer Model:FeCr25Al5
  • Resistivitas:1.42
  • Kapadhetan:7,25 g/cm3
  • lumahing:padhang / oksidasi / Golden / Blue
  • merek dagang:TANKII
  • Asal:Shanghai, China
  • Kode HS:722300
  • Kapasitas produksi:5000 Ton / Taun
  • Detail Produk

    FAQ

    Tag produk

    Resistance Wire digawe saka Nikel Chrome Alloys, Nikel Chrome Iron Alloys, Iron Chrome Aluminium Alloys, Tembaga Nikel Alloys.

    Utamane digunakake ing pemanas, unsur pemanas lan resistor, lsp.

    NiCr 80/20, NiCr 70/30, NiCr 60/15, NiCr 35/20

    FeCrAl15-5, FeCrAl20-5, FeCrAl 25-5, lsp...

    Constantan, Alloy 30, Alloy 60, Alloy 90, lsp.

    Resistivitas listrik saka 0,02 u ohm / m-1,53 u ohm / m

    Suhu operasi saka 200 C nganti 1400 C

    Pls bebas hubungi kita yen ana pitakonan.

    NiCr:
    RESISTOHM 20, RESISTOHM 30, RESISTOHM 40, RESISTOHM 60, RESISTOHM 70, RESISTOHM 80

    FeCrAl:
    RESISTOHM 125, RESISTOHM 135, RESISTOHM 140,
    RESISTOHM 145, RESISTOHM 153

    CuNi
    Constantan, Cuprothal 5, Cuprothal 10, Cuprothal 15, Cuprothal 30, Eurica

    FeCrAl Alloy Grade Komposisi kimia %
    C P S Mn Si Cr Ni Al Fe Re liyane
    maksimal (≤)
    1Cr13Al4 0.12 0,025 0,025 0.7 ≤1.00 12.5-15.0 —- 3.5-4.5 0.1 Bal.
    0Cr15Al5 0.12 0,025 0,025 0.7 ≤1.00 14.5-15.5 —- 4.5-5.3 0.1 Bal.
    0Cr25Al5 0.06 0,025 0,025 0.7 ≤0.60 23.0-26.0 ≤0.60 4.5-6.5 0.1 Bal.
    0Cr23Al5 0.06 0,025 0,025 0.7 ≤0.60 20.5-23.5 ≤0.60 4.2-5.3 0.1 Bal.
    0Cr21Al6 0.06 0,025 0,025 0.7 ≤1.00 19.0-22.0 ≤0.60 5.0-7.0 0.1 Bal.
    0Cr21Al4 0.06 0,025 0,025 0.7 ≤1.00 21.0-23.0 ≤0.60 3.0-5.2 0.1 Bal.
    0Cr21Al6Nb 0.05 0,025 0,025 0.7 ≤0.60 21.0-23.0 ≤0.60 5.0-7.0 0.1 Bal.
    0Cr27Al7Mo2 0.05 0,025 0,025 0.7 ≤0.40 26.5-27.8 ≤0.60 6.0-7.0 0.1 Bal.

    Komposisi lan Sifat Kimia:

    Properti / Kelas NiCr 80/20 NiCr 70/30 NiCr 60/15 NiCr 35/20 NiCr 30/20
    Kimia Utama
    Komposisi(%)
    Ni Bal. Bal. 55.0-61.0 34.0-37.0 30.0-34.0
    Cr 20.0-23.0 28.0-31.0 15.0-18.0 18.0-21.0 18.0-21.0
    Fe ≤ 1.0 ≤ 1.0 Bal. Bal. Bal.
    Max Kerja
    Suhu (ºC)
    1200 1250 1150 1100 1100
    Resistivitas ing 20ºC
    (μ Ω · m)
    1.09 1.18 1.12 1.04 1.04
    Kapadhetan (g/cm3) 8.4 8.1 8.2 7.9 7.9
    Konduktivitas Termal (KJ/m· h· ºC) 60.3 45.2 45.2 43.8 43.8
    Koefisien termal
    Ekspansi (α × 10-6/ºC)
    18 17 17 19 19
    Titik Lebur (ºC) 1400 1380 1390 1390 1390
    Elongasi (%) > 20 > 20 > 20 > 20 > 20
    Struktur Mikrografi austenit austenit austenit austenit austenit
    Sifat Magnetik nonmagnetik nonmagnetik nonmagnetik nonmagnetik nonmagnetik
    CuNi Alloys Grade Resistivitas listrik
    (20 derajatΩ
    mm² / m)
    koefisien suhu saka resistance
    (10^6/derajat)
    Kapadhetan
    g/mm²
    Maks. suhu
    (derajat)
    Titik lebur
    (derajat)
    CuNi1 0.03 < 1000 8.9 200 1085
    CuNi2 0.05 < 1200 8.9 200 1090
    CuNi6 0.10 < 600 8.9 220 1095
    CuNi8 0.12 < 570 8.9 250 1097
    CuNi10 0.15 < 500 8.9 250 1100
    CuNi14 0.20 < 380 8.9 300 1115
    CuNi19 0.25 < 250 8.9 300 1135
    CuNi22 0.30 < 160 8.9 300 1150
    CuNi30 0.35 < 100 8.9 350 1170
    CuNi34 0.40 -0 8.9 350 1180
    CuNi40 0.48 ± 40 8.9 400 1280
    CuNi44 0.50 < -6 8.9 400 1280