Komposisi Kimia
| Unsur | Komponen |
| Be | 1,85-2,10% |
| Co+Ni | 0,20% Minimal |
| Co+Ni+Fe | Maks. 0,60%. |
| Cu | Saldo |
Sifat Fisik Khas
| Kapadhetan (g/cm3) | 8.36 |
| Kapadhetan sadurunge pengerasan (g/cm3) | 8.25 |
| Modulus Elastis (kg/mm2 (103)) | 13.40 |
| Koefisien Ekspansi Termal (20 °C nganti 200 °C m/m/°C) | 17 x 10-6 |
| Konduktivitas Termal (kal/(cm-s-°C)) | 0.25 |
| Rentang Leleh (°C) | 870-980 |
Sifat mekanik (Sadurunge perawatan Pengerasan):
| status | Kekuwatan tarik (Kg/mm3) | Kekerasan (HV) | Konduktivitas (IACS%) | Pemanjangan (%) |
| H | 70-85 | 210-240 | 22 | 2-8 |
| 1/2 Jam | 60-71 | 160-210 | 22 | 5-25 |
| 0 | 42-55 | 90-160 | 22 | 35-70 |
Sawise perawatan pengerasan
| Merek | Kekuwatan tarik (Kg/mm3) | Kekerasan (HV) | Konduktivitas (IACS%) | Pemanjangan (%) |
| C17200-TM06 | 1070-1210 | 330-390 | ≥17 | ≥4 |
Fitur-fitur
1. Konduktivitas termal sing dhuwur
2. Tahan korosi sing dhuwur, utamane cocok kanggo cetakan produk polioksietilena (PVC).
3. Kekerasan, tahan aus, lan ketangguhan sing dhuwur, amarga sisipan sing digunakake karo baja cetakan lan aluminium bisa nggawe cetakan muter kanthi efisien banget, lan ndawakake umur layanan.
4. Performa polesan apik, bisa entuk presisi permukaan pangilon sing dhuwur lan desain bentuk sing rumit.
5. Tahan lengket sing apik, gampang dilas karo logam liyane, gampang diolah, ora perlu perawatan panas tambahan.
150 0000 2421