Paduan Fe-Cr-Al kanthi resistivitas lan suhu layanan sing luwih dhuwur tinimbang paduan NiCr lan uga duwe rega sing luwih murah. Aplikasi:
Steker listrik wesi-krom-aluminium digunakake kanthi apik kanggo nggawe elemen pemanas listrik ing peralatan rumah tangga lan peralatan industri, ron safety aplikasi khusus, mesin pengion, teater natera, cetakan plastimoulding, besi solder, elemen tubular berselubung logam, lan elemen kartrid. Kandungan Kimia % | Bahan paduan | Komposisi kimia% |
| C | P | S | Mn | Si | Cr | Ni | Al | Fe | Liyane |
| maksimal (≦) |
| 1Cr13Al4 | 0.12 | 0.0025 | 0.0025 | 0.7 | ≦1.00 | 12.5-15.0 | - | 3.5-4.5 | Ngaso | - |
| 0Cr15Al5 | 0.12 | 0.0025 | 0.0025 | 0.7 | ≦1.00 | 14.5-15.5 | - | 4.5-5.3 | Ngaso | - |
| 0Cr25Al5 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≦0.60 | 23.0-26.0 | ≦0.60 | 4.5-6.5 | Ngaso | - |
| 0Cr23Al5 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≦0.60 | 20.5-23.5 | ≦0.60 | 4.2-5.3 | Ngaso | - |
| 0Cr21Al6 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≦1.00 | 19.0-22.0 | ≦0.60 | 5.0-7.0 | Ngaso | - |
| 0Cr19Al3 | 0.06 | 0.0025 | 0.0025 | 0.7 | ≦1.00 | 18.0-21.0 | ≦0.60 | 3.0-4.2 | Ngaso | - |
| 0Cr21Al6Nb | 0.05 | 0.0025 | 0.0025 | 0.7 | ≦0.60 | 21.0-23.0 | ≦0.60 | 5.0-7.0 | Ngaso | Nb tambah 0.5 |
| 0Cr27Al7Mo2 | 0.05 | 0.0025 | 0.0025 | 0.2 | ≦0.40 | 26.5-27.8 | ≦0.60 | 6.0-7.0 | Ngaso | |
| Kelas | 1Cr13Al4 | TK1 | 0Cr25Al5 | 0Cr20Al6RE | 0Cr23Al5 | 0Cr19Al3 | 0Cr21Al6Nb | 0Cr27Al7Mo2 |
| Komposisi nominal% | Cr | 12.0-15.0 | 22.0-26.0 | 23.0-26.0 | 19.0-22.0 | 22.5-24.5 | 18.0-21.0 | 21.0-23.0 | 26.5-27.8 |
| Al | 4.0-6.0 | 5.0-7.0 | 4.5-6.5 | 5.0-7.0 | 4.2-5.0 | 3.0-4.2 | 5.0-7.0 | 6.0-7.0 |
| Re | sing cocog | 0.04-1.0 | sing cocog | sing cocog | sing cocog | sing cocog | sing cocog | sing cocog |
| Fe | Bal. | | Bal. | Bal. | Bal. | Bal. | Bal. | Bal. |
| | | | | | | Nb0.5 | Mo1.8-2.2 |
| Suhu operasi maksimal (°C) | 650 | 1400 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 |
| Resistivitas 20℃ (Ω/mm2/m) | 1.25 | 1.48 | 1.42 | 1.40 | 1.35 | 1.23 | 1.45 | 1.53 |
| Kapadhetan (g/cm³) | 7.4 | 7.1 | 7.1 | 7.16 | 7.25 | 7.35 | 7.1 | 7.1 |
| Konduktivitas Termal ing 20℃,W/(M·K) | 0.49 | 0.49 | 0.46 | 0.48 | 3.46 | 0.49 | 0.49 | 0.49 |
| Koefisien Ekspansi Linear (×10¯6/℃) 20-1000℃) | 15.4 | 16 | 16 | 14 | 15 | 13.5 | 16 | 16 |
| Titik Leleh Perkiraan (℃) | 1450 | 1520 | 1500 | 1500 | 1500 | 1500 | 1510 | 1520 |
| Kekuwatan Tarik (N/mm2) | 580-680 | 680-830 | 630-780 | 630-780 | 630-780 | 600-700 | 650-800 | 680-830 |
| Pemanjangan (%) | ›16 | ›10 | ›12 | ›12 | ›12 | ›12 | ›12 | ›10 |
| Tingkat Penyusutan Variasi Bagian (%) | 65-75 | 65-75 | 60-75 | 65-75 | 65-75 | 65-75 | 65-75 | 65-75 |
| Frekuensi Bend Bola-bali (F/R) | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 | ›5 |
| Kekerasan (HB) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 |
| Struktur Mikrografik | Ferit | Ferit | Ferit | Ferit | Ferit | Ferit | Ferit | Ferit |
| Sifat Magnetik | Magnetik | Magnetik | Magnetik | Magnetik | Magnetik | Magnetik | Magnetik | Magnetik |
| Urip Cepet (h/℃) | no | ≥80/1350 | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥50/1350 | ≥50/1350 |
Sadurunge: Kawat Semprotan Termal NiCr 80/20 kanggo Penyemprotan Busur: Solusi Pelapisan Kinerja Tinggi Sabanjure: Paduan Nikel Hastelloy C276 Ernicrmo-4 Las MIG TIG Las Inconel C-276 Kawat C22, B3, B2