Standar: AWS A5.10 ER4043 | Komposisi kimia % | ||||||||||
Si | Fe | Cu | Mn | Zn | Liyane | AL | |||||
sasmita ER4043 | 4.5 - 6.0 | ≤ 0,80 | ≤ 0.30 | ≤ 0,05 | ≤ 0.10 | - | Ngaso | ||||
Jinis | Spool (MIG) | Tabung (TIG) | |||||||||
Spesifikasi (MM) | 0.8,0.9,1.0,1.2,1.6,2.0 | 1.6,2.0,2.4,3.2,4.0,5.0 | |||||||||
Paket | S100/0.5kg S200/2kg S270,S300/6kg-7kg S360/20kg | 5kg / kothak 10kg / kothak dawa: 1000MM | |||||||||
Sifat Mekanik | Suhu Fusion ºC | listrik IACS | Kapadhetan g/mm3 | Tarik Mpa | ngasilaken Mpa | Elongation % | |||||
575 - 630 | 42% | 2.68 | 130 - 160 | 70 - 120 | 10 - 18 | ||||||
Dhiameter (MM) | 1.2 | 1.6 | 2.0 | ||||||||
MIG Welding | Arus Las – A | 180 - 300 | 200 - 400 | 240 - 450 | |||||||
Tegangan Las - V | 18 - 26 | 20 - 28 | 22 - 32 | ||||||||
TIG Welding | Dhiameter (MM) | 1.6 - 2.4 | 2.4 - 4.0 | 4.0 - 5.0 | |||||||
Arus Las – A | 150 - 250 | 200 - 320 | 220 - 400 | ||||||||
Aplikasi | Dianjurake kanggo welding 6061,6XXX seri;3XXXand2XXX seri aluminium alloy. | ||||||||||
Kabar | 1,Prodhuk bisa katahan kanggo rong taun ing kondisi packing pabrik lan nutup, lan packing bisa dibusak telung sasi ing lingkungan atmosfer biasanipun. 2,Produk kudu disimpen ing ventilated, garing lan Panggonan. 3, Sawise kabel dibusak saka paket, disaranake tutup bukti bledug cocok |
Almunium alloy welding seri:
Item | AWS | Komposisi Kimia Paduan Aluminium(%) | |||||||||
Cu | Si | Fe | Mn | Mg | Cr | Zn | Ti | AL | |||
Aluminium Murni | ER1100 | 0.05-0.20 | 1.00 | 0.05 | 0.10 | 99.5 | |||||
Plastisitas apik, kanggo welding protèktif gas utawa welding busur argon saka aluminium murni tahan karat. | |||||||||||
Aluminium Alloy Kab | ER5183 | 0.10 | 0.40 | 0.40 | 0.50-1.0 | 4.30-5.20 | 0.05-0.25 | 0.25 | 0.15 | Rem | |
kekuatan dhuwur, resistance karat apik, kanggo welding argon busur. | |||||||||||
ER5356 | 0.10 | 0.25 | 0.40 | 0.05-0.20 | 4.50-5.50 | 0.05-0.20 | 0.10 | 0.06-0.20 | Rem | ||
kekuatan dhuwur, resistance karat apik, kanggo welding argon busur. | |||||||||||
ER5087 | 0.05 | 0.25 | 0.40 | 0.70-1.10 | 4.50-5.20 | 0.05-0.25 | 0.25 | 0.15 | Rem | ||
resistance karat apik, weldability lan plasticity, kanggo welding protèktif gas utawa welding argon busur. | |||||||||||
ER4047 | 0.30 | 11.0-13.0 | 0.80 | 0.15 | 0.10 | 0.20 | Rem | ||||
Utamane kanggo brazing lan soldering. | |||||||||||
ER4043 | 0.30 | 4.50-6.00 | 0.80 | 0.05 | 0.05 | 0.10 | 0.20 | Rem | |||
resistance karat apik, aplikasi sudhut, protèktif gas utawa argon acr welding. | |||||||||||
Nikel Welding seri:
ERNiCrMo-3,ERNiCrMo-4,ERNiCrMo-13,ERNiCrFe-3,ERNiCrFe-7,ERNiCr-3,ERNiCu-7,ERNiCu-7,ERNi-1
Standar:Selaras karo Sertifikasi AWS A5.14 ASME SFA A5.14
Ukuran: 0.8 MM / 1.0 MM / 1.2 MM / 1.6 MM / 2.4 MM / 3.2 MM / 3.8 MM / 4.0 MM / 5.0 MM
Formulir: MIG (15kgs/spool), TIG (5kgs/box)