| Standar: AWS A5.10 ER4043 | Komposisi Kimia % | ||||||||||
| Si | Fe | Cu | Mn | Zn | Liyane | AL | |||||
| Kelas ER4043 | 4.5 - 6.0 | ≤ 0.80 | ≤ 0.30 | ≤ 0,05 | ≤ 0.10 | - | Ngaso | ||||
| Tipe | Gulungan (MIG) | Tabung (TIG) | |||||||||
| Spesifikasi (MM) | 0.8,0.9,1.0,1.2,1.6,2.0 | 1.6, 2.0, 2.4, 3.2, 4.0, 5.0 | |||||||||
| Paket | S100/0.5kg S200/2kg S270, S300/6kg-7kg S360/20kg | 5kg/kothak 10kg/kothak dawane: 1000MM | |||||||||
| Sifat Mekanik | Suhu Fusi ºC | Listrik IACS | Kapadhetan g/mm3 | Tarik Mpa | Asil panen Mpa | Pemanjangan % | |||||
| 575 - 630 | 42% | 2.68 | 130 - 160 | 70 - 120 | 10 - 18 | ||||||
| Diameter (MM) | 1.2 | 1.6 | 2.0 | ||||||||
| MIG Pengelasan | Arus Pengelasan – A | 180 - 300 | 200 - 400 | 240 - 450 | |||||||
| Tegangan Pengelasan- V | 18 - 26 | 20 - 28 | 22 - 32 | ||||||||
| TIG Pengelasan | Diameter (MM) | 1.6 - 2.4 | 2.4 - 4.0 | 4.0 - 5.0 | |||||||
| Arus Pengelasan – A | 150 - 250 | 200 - 320 | 220 - 400 | ||||||||
| Aplikasi | Disaranake kanggo ngelas 6061, seri 6XXX; paduan aluminium seri 3XXX lan 2XXX. | ||||||||||
| Kabar | 1, Produk kasebut bisa disimpen nganti rong taun miturut kondisi kemasan pabrik lan disegel, lan kemasan bisa dicopot sajrone telung sasi ing lingkungan atmosfer biasane. 2, Produk kudu disimpen ing panggonan sing berventilasi, garing lan adhem. 3, Sawise kawat dicopot saka paket, disaranake tutup anti bledug sing cocog | ||||||||||
Almunium alloy welding seri:
| Barang | AWS | Kompositasi Kimia Paduan Aluminium (%) | |||||||||
| Cu | Si | Fe | Mn | Mg | Cr | Zn | Ti | AL | |||
| Aluminium Murni | ER1100 | 0.05-0.20 | 1.00 | 0.05 | 0.10 | 99.5 | |||||
| Plastisitas apik, kanggo pengelasan pelindung gas utawa pengelasan busur argon saka aluminium murni sing tahan korosi. | |||||||||||
| Paduan Aluminium | ER5183 | 0.10 | 0.40 | 0.40 | 0.50-1.0 | 4.30-5.20 | 0.05-0.25 | 0.25 | 0.15 | Rem | |
| Kekuwatan dhuwur, tahan korosi sing apik, kanggo pengelasan busur argon. | |||||||||||
| ER5356 | 0.10 | 0.25 | 0.40 | 0.05-0.20 | 4.50-5.50 | 0.05-0.20 | 0.10 | 0.06-0.20 | Rem | ||
| Kekuwatan dhuwur, tahan korosi sing apik, kanggo pengelasan busur argon. | |||||||||||
| ER5087 | 0.05 | 0.25 | 0.40 | 0.70-1.10 | 4.50-5.20 | 0.05-0.25 | 0.25 | 0.15 | Rem | ||
| Tahan korosi, kemampuan las, lan plastisitas sing apik, kanggo pengelasan pelindung gas utawa pengelasan busur argon. | |||||||||||
| ER4047 | 0.30 | 11.0-13.0 | 0.80 | 0.15 | 0.10 | 0.20 | Rem | ||||
| Utamane kanggo nyolder lan matri. | |||||||||||
| ER4043 | 0.30 | 4.50-6.00 | 0.80 | 0.05 | 0.05 | 0.10 | 0.20 | Rem | |||
| Tahan korosi sing apik, aplikasi sing jembar, kanggo pengelasan pelindung gas utawa argon acr. | |||||||||||
Seri Pengelasan Nikel:
ERNiCrMo-3,ERNiCrMo-4,ERNiCrMo-13,ERNiCrFe-3,ERNiCrFe-7,ERNiCr-3,ERNiCu-7,ERNiCu-7,ERNi-1
Standar:Sesuai karo Sertifikasi AWS A5.14 ASME SFA A5.14
Ukuran: 0.8MM / 1.0MM / 1.2MM / 1.6MM / 2.4MM / 3.2MM / 3.8MM / 4.0MM / 5.0MM
Wangun: MIG (15kgs/spool), TIG (5kgs/box)
| Tipe | Standar | Komposisi kimia Manin % | Aplikasi khas |
| Kawat las nikel | A5.14 ERNi-1 | Ni ≥ 93 Ti3 Al1 Cr– Mo– | ERNi-1 digunakake kanggo pengelasan GMAW, GTAW lan ASAW saka Nikel 200 lan 201, nggabungake paduan kasebut karo baja tahan karat lan karbon, lan logam dasar nikel lan tembaga-nikel liyane. Uga digunakake kanggo nutupi baja. |
| Kawat las NiCulding | A5.14 ERNiCu-7 | Ni 65 Cr– Mo– Ti2 Liyane: Cu | ERNiCu-7 kuwi kawat dasar paduan tembaga-nikel kanggo pengelasan GMAW lan GTAW saka paduan Monel 400 lan 404. Uga digunakake kanggo nutupi baja. sawise pisanan ngetrapake Lapisan nikel 610. |
| Kawat las CuNi | A5.7 ERCuNi | Ni 30 Cr– Mo– Liyane: Cu | ERCuNi digunakake kanggo pengelasan busur gas logam lan gas tungsten. Uga bisa digunakake kanggo pengelasan oxy-fuel tembaga 70/30, 80/20, lan 90/10. paduan nikel. Lapisan penghalang paduan nikel 610 dianjurake sadurunge nutupi baja nganggo proses las GMAW. |
| NiCr kawat las | A5.14 ERNiCrFe-3 | Ni≥ 67 Cr 20 Mo— Mn3 Nb2.5 Fe2 | Elektroda tipe ENiCrFe-3 digunakake kanggo ngelas paduan nikel-kromium-besi karo awake dhewe lan kanggo ngelas sing beda antarane paduan lan baja nikel-kromium-wesi utawa baja tahan karat. |
| A5.14 ERNiCrFe-7 | Ni: Sisa Cr 30 Fe 9 | Tipe ERNiCrFe-7 digunakake kanggo pengelasan gas-tungsten-arc lan gas-logam-arc saka INCONEL 690. | |
| Kawat las NiCrMo | A5.14 ERNiCrMo-3 | Ni≥ 58 Cr 21 Mo 9 Nb3.5 Fe ≤1.0 | ERNiCrMo-3 digunakake utamane kanggo busur gas tungsten lan logam gas lan logam dasar sing cocog karo komposisi. Iki uga digunakake kanggo ngelas. Inconel 601 lan Incoloy 800. Iki bisa digunakake kanggo ngelas kombinasi logam sing beda-beda kayata baja, baja tahan karat, Inconel lan Paduan incoloy. |
| A5.14 ERNiCrMo-4 | Ni Rest Cr 16 Mo 16 W3.7 | ERNiCrMo-4 digunakake kanggo ngelas bahan dasar nikel-kromium-molibdenum kanggo awake dhewe, baja lan paduan dasar nikel liyane lan kanggo baja pelapis. | |
| A5.14 ERNiCrMo-10 | Ni Sisa Cr 21 Mo 14 W3.2 Fe 2.5 | ERNiCrMo-10 digunakake kanggo ngelas bahan dasar nikel-kromium-molibdenum, baja lan paduan dasar nikel liyane, lan kanggo baja cladding. Bisa digunakake kanggo ngelas baja tahan karat duplex, super duplex. | |
| A5.14 ERNiCrMo-14 | Ni Rest Cr 21 Mo 16 W3.7 | ERNiCrMo-14 digunakake kanggo pengelasan gas-tungsten-arc lan gas-logam-arc saka baja tahan karat dupleks, super-dupleks lan super-austenitik, uga paduan nikel kayata UNS N06059 lan N06022, paduan INCONEL C-276, lan paduan INCONEL 22, 625, lan 686. |

150 0000 2421