Konten kimia,%
Ni | Mn | Fe | Si | Cu | Liyane | Arahan rohs | |||
Cd | Pb | Hg | Cr | ||||||
44 | 1,50% | 0,5 | - | Bal | - | ND | ND | ND | ND |
Properties Teknik
Temp Maksimal Layanan Tanduran | 400ººC |
Resisivitas ing 20ºC | 0.49 ± 5% ohm mm2 / m |
Kapadhetan | 8.9 g / cm3 |
Konduktivitas termal | -6 (max) |
Titik lebur | 1280ºc |
Kekuwatan tensile, N / MM2 anneeled, alus | 340 ~ 535 MPA |
Kekuwatan tensile, n / mm3 kadhemen digulung | 680 ~ 1070 MPA |
Elongasi (Anneal) | 25% (min) |
Elongasi (kadhemen digulung) | ≥min) 2% (min) |
Emf vs, μV / ºc (0 ~ 100ºC) | -43 |
Struktur micrographic | Austenite |
Properti Magnetik | Non |